Single-component coating formulas were prepared by dissolving ChDs into water at neutral pH. A concentration of 10 g/L was established for all chitosan derivatives, based on solubility tests. Two-component coating formulas with total solids content of 1.33% were prepared by mechanical dispersion of the MFC suspension into ChD-solution, at MFC:ChD ratio of 1:1